A study of the surface analysis of some water-soluble polymers by inverse gas chromatography


Askin A., TOPALOĞLU YAZICI D.

Surface and Interface Analysis, cilt.40, sa.9, ss.1237-1241, 2008 (SCI-Expanded, Scopus) identifier identifier

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 40 Sayı: 9
  • Basım Tarihi: 2008
  • Doi Numarası: 10.1002/sia.2869
  • Dergi Adı: Surface and Interface Analysis
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus
  • Sayfa Sayıları: ss.1237-1241
  • Anahtar Kelimeler: inverse-gas chromatography, surface energy, acid-base surface characteristics, water-soluble diblock copolymer, COPOLYMERS, INTERFACE, BLENDS
  • Eskişehir Osmangazi Üniversitesi Adresli: Evet

Özet

The surface characterization of 2-(dimethylamino)ethylmethacrylate (DMA) and 2-(N-morpholino)ethylmethacrylate (MEMA) homopolymers and DMA-MEMA diblock copolymer was studied using inverse-gas chromatography (IGC). The analyzed surface properties of (co)polymers were the dispersive component of the surface energy (ysd) and the acid - base characters of (co)polymer surfaces. The specific free energy (ΔGsp), enthalpy (ΔHsp), and entropy (ΔSsp) of adsorption of polar probes on (co)polymers were calculated. The values of ΔH sp were correlated with both the donor and the modified acceptor numbers (AN) of the probes to quantify the acidic KA and the basic KD parameters of (co)polymer surfaces. The values obtained for the KA and KD parameters indicated basic characters for the surface of (co)polymers. The dispersive component values of the surface energy and the acid-base surface parameters of the DMA-MEMA diblock copolymer surface were found to be between those homopolymers as expected. Copyright © 2008 John Wiley & Sons, Ltd.