THE IMPORTANCE OF ZETA POTENTIAL MEASUREMENT IN THE FLOTATION OF DIASPORA AND CALCIUM MINERALS


Gürsoy Y. H., Filar A., Umucu Y.

20th Balkan Mineral Processing Congress, İstanbul, Türkiye, 9 - 11 Nisan 2026, cilt.1, ss.897-912, (Tam Metin Bildiri)

  • Yayın Türü: Bildiri / Tam Metin Bildiri
  • Cilt numarası: 1
  • Basıldığı Şehir: İstanbul
  • Basıldığı Ülke: Türkiye
  • Sayfa Sayıları: ss.897-912
  • Eskişehir Osmangazi Üniversitesi Adresli: Evet

Özet

The combined consideration of particle size and the collector effect is crucial for understanding the

flotation mechanism. In fine particles, an increase in surface area can increase collector adsorption,

leading to larger changes in zeta potential. However, in very fine particles, surface hydration and

electrostatic repulsion forces can increase, making bubble-particle binding more difficult. In larger

particles, the surface area decreases, limiting collector adsorption and resulting in smaller changes in

zeta potential. Therefore, both surface charge differences and collector adsorption become more

pronounced within the optimum particle size range.

The variation of zeta potential depending on particle size and collector type is a significant indicator of

flotation selectivity in the removal of calcium-based minerals from bauxite. Anionic collectors have

stronger adsorption, especially on carbonate minerals, which makes the zeta potential more negative.

Cationic collectors, on the other hand, can change the surface charge of minerals in the opposite

direction. As particle size decreases, the increase in surface area makes these effects more

pronounced. Therefore, zeta potential data is used as an important evaluation criterion for optimizing

flotation conditions and selecting the appropriate collector type in bauxite ores (Somasundaran, 1975;

Fuerstenau, 2005).

The removal of calcium-origin minerals (primarily calcite and dolomite) from diasporic bauxite ores

represents a significant challenge in the alumina industry, particularly for the Bayer process where

calcium impurities cause substantial operational difficulties. This comprehensive review examines the

pivotal role of zeta potential measurements in understanding and optimizing the flotation separation of

these mineral systems. The electrokinetic properties of diaspora [AlO(OH)] and associated calcium

minerals govern collector adsorption mechanisms, selectivity, and overall flotation performance.

Through critical analysis of recent literature and fundamental surface chemistry principles, this paper

demonstrates that zeta potential serves as an indispensable tool for reagent selection, pH optimization,

and process control. The distinct isoelectric points of diaspora (pH 5.0–7.5) and calcium minerals (pH

7.0–8.5) provide the theoretical basis for selective separation, while zeta potential measurements

enable quantitative verification of surface interactions.

This review presents the electrokinetic principles, collector-mineral interactions, depressant mineral

mechanisms, and the effects of grain size on zeta potential, offering a framework for future research

directions in this critical field.